J. Bidulská, R. Bidulský, M. Actis Grande
EFFECT OF NEW TYPE HEAT TREATMENT ON WEAR CHARACTERISTICS OF HIGH-STRENGTH SINTERED STEELS
K. s.: high-strength steel|heat treatment|sinter hardening|sliding wear|
No 3 (2010), p. 146-150
  mag01.pdf (345 kB)
mag01.txt (1 kB)  

J. Trpčevská, B. Hlucháňová, T. Vindt, W. Zorawski, D. Jakubéczyová
CHARACTERIZATION OF THE BOTTOM DROSS FORMED DURING BATCH HOT-DIP GALVANIZING AND ITS REFINING
K. s.: galvanization|microstructure|intermetallics|X-ray diffraction|dross formation|refining|
No 3 (2010), p. 151-156
  mag02.pdf (646 kB)
mag02.txt (897 B)  

M. Hagarová, I. Štěpánek, D. Jakubéczyová
EVALUATION OF THIN PVD COATINGS BY ADHESIVE - COHESIVE TEST
K. s.: PVD|ARC|LARC|nanocomposite coatings|scratch test|
No 3 (2010), p. 157-164
  mag03.pdf (267 kB)
mag03.txt (960 B)  

T. Borovský, J. Kijac, M. Domovec
THE SLAG COMPOSITION INFLUENCE ON THE DEPHOSPHORIZATION AND ON THE LIFETIME OF ELECTRIC ARC FURNACE HEARTH REFRACTORY LINING
K. s.: electric arc furnace|dephosphorization|refractory wear|steel|slag|
No 3 (2010), p. 165-171
  mag04.pdf (258 kB)
mag04.txt (679 B)  

V. Rusňáková, J. Kijac, G. Grimplini, G. Rusňák
ANALYSIS OF SLAG IN MOLD UNDER STANDARD CONDITIONS AND IN CASE OF STICKER TEMPERATURE ALARM OCCURENCE
K. s.: casting|interstitial free (IF) steels|casting powder|slag viscosity|break temperature|
No 3 (2010), p. 172-180
  mag05.pdf (255 kB)
mag05.txt (716 B)  

P. Gavendová, F. Kováč, V. Stoyka, I. Petryshynets, T. Kvačkaj
EFFECT OF TEMPER ROLLING ON THE STRAIN HARDENING OF A NON-ORIENTED ELECTROTECHNICAL STEEL
K. s.: microhardness|strain hardening|cold rolling|hot rolling|
No 3 (2010), p. 181-185
  mag06.pdf (50 kB)
mag06.txt (669 B)  

H. Lukáčová, B. Plešingerová, M. Vojtko, G. Bán
ELECTROCHEMICAL TREATMENT OF Ti6Al4V (1. PART)
K. s.: surface treatment|Ti6Al4V-alloy|electrochemical oxidation|
No 3 (2010), p. 186-193
  mag07.pdf (1 MB)
mag07.txt (628 B)  

A.A. Baba, F.A. Adekola, G.D. Ewuloye
LEACHING OF LEAD FROM SPENT MOTORCYCLE BATTERY IN HYDROCHLORIC ACID. PART I: DISSOLUTION KINETICS
K. s.: leaching|dissolution|spent batteries|hydrochoric acid|
No 3 (2010), p. 194-204
  mag08.pdf (444 kB)
mag08.txt (1 kB)